Hull after laminate repair complete 
Complete hull was given 1 thin epoxy penetrating coat, 1 thick coat epoxy followed with a layer of Xynole Poliester Flexible Cloth, and then given 2 more thick coats of epoxy. The hull was then furnished wit 2 more white epoxy barrier coats. All within a time period to achieve chemical bonding. Only high quality non blushing epoxy materials where used.